Not sure what I am doing wrong here. Applying the WTF to smaller projects is no problem, but I cannot get it to work well on a larger project. I have turned a platter about 18" diameter and cannot make a decent finish. I cannot get the towel marks out, either rotary if applied on the lathe or linear if applied manually. If I continue to work it until The marks flatten, it is too close to dry and leaves a rough finish. I even tried spraying it on with my airbrush, both straight from the can and thinned. Some areas come out perfect and others are stippled, appearing like it is beading upon the underlying finish (that would be cured WTF sanded with 400 paper).
What am I doing wrong? The product just appeared too good initially.
david