Hey All,
I have put on three coats of Watco Satin Spray Lacquer on stained Oak cabinet doors, waiting the recommended two hours before re-coating and the finish always dries with white streaks. I always used Deft spray sating lacquer before and never had problems, I even sanded with 320 before reocat the last time and still white streaks. Any ideas? The temperature might have been 63-65, but no cooler.